Why molecules matter: polymers in fibres
This chapter assumes you know the three fibre families (natural, regenerated, synthetic) and the idea of a fibre as a thin, long strand that is spun into yarn. School-level chemistry helps. It explains the molecular structure behind the properties covered in the next chapter.
Fibres are made of polymers
A polymer is a very long molecule built by joining many small repeating units, called monomers, into a chain. Every textile fibre is made mostly of polymer chains. The kind of chain decides most of what a fibre does.
Three features of the chain matter most:
- Chemical groups along the chain. Some groups attract water (polar groups such as -OH, -NH and -COOH). Others repel it (hydrocarbon sections).
- Chain length. Longer chains give stronger fibres, because more of each chain is held by its neighbours.
- Chain arrangement. Chains can lie in neat, parallel, tightly packed regions or in tangled, loose regions.
| Fibre | Polymer | Repeating unit type | Key groups |
|---|---|---|---|
| Cotton, linen, viscose | Cellulose | Glucose rings | Many -OH groups |
| Wool, silk | Protein (keratin, fibroin) | Amino acids | Amide links, side groups |
| Polyester (PET) | Polyethylene terephthalate | Ester units | Ester links, benzene rings |
| Nylon 6,6 | Polyamide | Amide units | Amide links, short carbon chains |
| Acrylic | Polyacrylonitrile (at least 85% by mass) | Acrylonitrile | Nitrile groups |
| Elastane | Segmented polyurethane | Soft and hard blocks | Urethane links |
Bonds inside and between chains
Two kinds of bonding matter, and confusing them is a common error.
Covalent bonds hold atoms together along a chain. They are strong. Ordinary wear, washing and ironing do not break them, though strong bleach, hot alkali or ultraviolet light can.
Intermolecular forces act between neighbouring chains. They are much weaker, but there are very many of them. Fibre behaviour is mostly decided here. The main types are:
- Hydrogen bonds. An attraction between a hydrogen atom on one polar group and an oxygen or nitrogen atom on another. Cellulose and nylon form many.
- Van der Waals forces. Weak attractions between any closely packed chains. Polyester and acrylic rely on these more.
- Ionic (salt) bridges and disulfide bonds. Found in wool. Disulfide bonds are covalent cross-links between sulfur atoms on neighbouring protein chains.
Water and heat act on the weak forces. Water molecules can slip between chains and replace hydrogen bonds. Heat gives chains enough energy to move. This is why fibres change shape when wet or hot, while the chains themselves stay intact.
Crystalline and amorphous regions
Within a fibre, chains are not uniformly arranged. Two kinds of region exist side by side:
- Crystalline (ordered) regions. Chains lie parallel and packed closely. Neighbouring chains bond strongly. These regions are strong, stiff and hard for water to enter.
- Amorphous (disordered) regions. Chains are tangled and loosely packed. These regions stretch more and let water and dyes enter.
The ratio of the two, and how well the chains are aligned along the fibre axis (orientation), explains many differences.
| Property | More crystalline and oriented | More amorphous |
|---|---|---|
| Strength | Higher | Lower |
| Stiffness | Higher | Lower |
| Moisture absorption | Lower | Higher |
| Dye uptake | Slower | Faster |
Cotton is a good example. It is about 70% crystalline cellulose, and its strength increases slightly when wet. The reason is that water swells the amorphous regions and lets the chains share load more evenly. Viscose is a second example. It has the same chemical polymer as cotton, but its chains are shorter and less crystalline, so it is weaker, and it loses much more strength when wet.
Worked example: why cotton absorbs and polyester does not
Cellulose has three -OH groups on each glucose ring. These groups form hydrogen bonds with water. Cotton therefore takes up about 7 to 8.5% of its dry mass as moisture at standard conditions (65% relative humidity, 20 °C). This is its moisture regain, a property the next chapter defines fully.
Polyester (PET) has ester links and benzene rings and few polar groups that can bond to water. Its standard regain is about 0.4%. Water stays on the surface and between yarns rather than entering the fibre.
Consequences follow from the chemistry:
- Cotton feels damp and dries slowly, because water is held inside the fibre.
- Polyester dries quickly, because there is almost no water inside to remove.
- Polyester can build up static charge, because it cannot carry charge away through absorbed moisture.
- Polyester resists water-based dyes. It is dyed with disperse dyes at high temperature (typically around 130 °C under pressure) so the dye can enter its tight structure.
- Polyester attracts oily stains more easily than cotton, because it is oleophilic (oil-attracting).
Shape memory and heat: the glass transition and melting
Synthetic fibres are thermoplastic: they soften when heated and harden on cooling. Two temperatures describe this.
- Glass transition temperature (Tg). Below it, chains in amorphous regions are frozen in place. Above it, they can move. For polyester Tg is about 70 to 80 °C, and for nylon 6,6 it is about 50 °C when dry (lower when wet).
- Melting point (Tm). Where crystalline regions break down. Polyester melts at about 255 °C and nylon 6,6 at about 255 to 265 °C. Acrylic does not melt cleanly and decomposes first.
Heat setting uses this. A fabric is held in shape and heated above Tg but below Tm, then cooled. The chains lock into the new arrangement, which gives lasting pleats and dimensional stability. The same mechanism means a hot wash or iron above Tg can set in wrinkles or distort the fabric.
Natural fibres behave differently. Cellulose and protein do not melt. They char or burn. Cotton tolerates ironing at around 200 °C, while wool and silk are damaged at lower temperatures.
Why elastane stretches: block structure
Most fibres stretch only 2 to 30% before breaking or deforming. Elastane stretches 400 to 700% and recovers. The reason is its segmented structure.
- Soft segments are long, flexible, coiled chains. They uncoil when stretched.
- Hard segments are short, rigid blocks that pack together and act as physical cross-links, anchoring the soft chains.
When you release the fibre, the soft segments coil back and the hard segments hold the network together. Wool shows a related effect. Its protein chains are folded in a spring-like helix (the alpha helix) and cross-linked by disulfide bonds, so wool can stretch and recover. Wool recovers well from small stretches but can be permanently set when stretched wet and dried.
Chain length and degree of polymerisation
The degree of polymerisation (DP) is the number of repeating units in a chain. It is a rough measure of chain length.
- Native cotton cellulose has a DP of about 2,000 to 10,000.
- Viscose has a DP of about 250 to 500, because the manufacturing process breaks chains.
- Lyocell and modal have a higher DP than standard viscose, and that is one reason they are stronger when wet.
Chemical damage shortens chains. Chlorine bleach and acid attack cellulose, and the fabric loses strength. Alkali and chlorine bleach attack protein fibres such as wool and silk. This is why care labels restrict bleach for some fibres.
Common errors
- Saying natural fibres are "just cellulose". Wool and silk are proteins. Their chemistry and care differ completely.
- Treating cotton and viscose as the same. They share the same repeating unit, but chain length and crystallinity differ, so wet strength and drying behaviour differ.
- Assuming a stronger covalent bond means a stronger fibre. Chain alignment and intermolecular forces matter at least as much.
- Assuming fibres melt in the wash. Washing temperatures are below Tm, but they can exceed Tg, which is enough to change shape.
Summary of cause and effect
| Molecular feature | Fibre-level effect | Example |
|---|---|---|
| Many -OH or polar groups | High moisture regain, slow drying | Cotton, viscose |
| Few polar groups | Low regain, quick drying, static | Polyester, acrylic |
| High crystallinity and orientation | Strength, stiffness | Linen, nylon |
| Disulfide cross-links and helical chains | Elastic recovery, crease resistance | Wool |
| Soft and hard segments | Very high stretch | Elastane |
| Thermoplastic chains | Heat setting, melting | Polyester, nylon |
| Short chains (low DP) | Weakness when wet | Standard viscose |
Exercise
Cotton and viscose are both cellulose, yet a wet viscose shirt is much weaker than a wet cotton shirt. Explain this using chain length and crystallinity.
Show answer
Cotton chains are very long (DP about 2,000 to 10,000) and form highly crystalline, oriented regions that hold the fibre together. Viscose is regenerated, which shortens the chains (DP about 250 to 500) and leaves less crystalline structure. When water enters and breaks hydrogen bonds between chains, viscose has fewer and shorter-range bonding regions left to carry load, so it loses much more strength. In cotton, water swells the amorphous regions and the long, crystalline chains still carry the load.
Exercise
A polyester dress is pressed with an iron at 200 °C, and the surface turns shiny and flat. Using Tg and Tm, explain what happened and why a cotton dress would not show the same damage at this temperature.
Show answer
Polyester has a Tg of about 70 to 80 °C and a Tm of about 255 °C. At 200 °C the iron is far above Tg and approaching Tm, so chains in the fibre become mobile and the fibres soften and fuse into a flattened, glossy surface that sets as it cools. Cotton is cellulose, which does not soften or melt. It tolerates ironing at around 200 °C, so it does not show this damage.
Exercise
Why do polyester garments hold oily stains and build static more than cotton ones?
Show answer
Polyester has few polar groups and a regain of about 0.4%, so it absorbs almost no water. Without absorbed moisture, charge cannot leak away, so static builds up. The fibre is oleophilic (attracts oils), and oily soil is not easily lifted by water-based washing. Cotton's many -OH groups hold water, which carries off charge and helps water-based washing work.