Sub topic 4
The properties that decide how a fibre wears
This chapter assumes you know the three fibre families (natural, regenerated, synthetic) and the idea that fibres are long-chain polymers. It also assumes you know the path from fibre to yarn to fabric. Here we turn molecular structure into the practical properties you will use in every later chapter: moisture regain, strength, elasticity, and heat behaviour.
Why a short list of properties is enough
A garment fails or succeeds in a few ways. It feels clammy or dry. It tears, pills or wears through. It bags at the knees or springs back. It shrinks, scorches or melts in the wash and iron. Four fibre properties explain most of this:
- Moisture behaviour
- Strength and durability
- Elasticity and recovery
- Heat behaviour
Fabric construction, yarn twist and finishing change the result. The fibre sets the starting point.
Moisture behaviour
Moisture regain
Moisture regain is the mass of water a fibre holds, as a percentage of its dry mass, when it sits in standard air (conventionally 65% relative humidity at 20 °C). It is measured on the fibre at rest in air. It is not how much water a wet fabric can soak up.
The cause is chemical. Fibres with many polar groups, such as hydroxyl (-OH) in cellulose and amide or amino groups in wool, attract water molecules. Fibres built from non-polar chains, such as polyester, have few places for water to bind.
| Fibre | Approximate regain at 65% RH |
|---|---|
| Wool | 13–16% |
| Viscose | 11–13% |
| Linen | 10–12% |
| Silk | 9–11% |
| Cotton | 7–8.5% |
| Nylon | 4–4.5% |
| Acrylic | 1.5–2% |
| Polyester | 0.4% |
Published figures vary by source and test conditions, so treat these as ranges.
What regain changes in wear
- Comfort in humid conditions. High-regain fibres take up vapour from the skin, which slows the build-up of clamminess.
- Static. Water on the surface lets charge leak away. Low-regain fibres such as polyester and acrylic build up static and cling.
- Drying time. Low-regain fibres dry quickly because little water sits inside them. Cotton dries slowly because it holds water inside the fibre and between fibres.
- Dyeing. Fibres that swell in water take up dyes more readily. Polyester needs disperse dyes and high temperature.
- Strength change when wet. Water acts as a plasticiser inside the fibre. In most fibres it also changes strength, as the next section shows.
Wicking is a different thing
Wicking is the movement of liquid water along fibre surfaces and through the spaces between fibres. A polyester fabric can wick well and have a regain near zero. Do not describe it as "absorbent" or "breathable" on the basis of regain alone. Sweat leaves a polyester sports shirt by capillary movement. It leaves a cotton shirt partly by absorption.
Strength and durability
Tenacity
Tenacity is the force a fibre can bear before it breaks, divided by its linear density. It is given in cN/tex or g/denier, so thick and thin fibres compare fairly. Tenacity is a breaking property. It does not tell you how well a fabric resists abrasion.
Strength comes from two features of the polymer: long chains, and chains packed in parallel with strong attraction between them. Highly oriented, crystalline regions carry load well. Amorphous regions are weaker and take up water and dye.
| Fibre | Dry tenacity (relative) | Wet versus dry strength |
|---|---|---|
| Nylon | High | About 85–90% of dry |
| Polyester | High | About 100% |
| Linen | High | Stronger wet |
| Cotton | Medium | Stronger wet (about 105–110%) |
| Silk | Medium to high | About 80–85% |
| Wool | Low | About 75–85% |
| Viscose | Low to medium | About 50–60% |
| Acrylic | Low to medium | About 90–100% |
Two points stand out. First, cotton and linen gain strength when wet, which suits repeated hot washing. Second, ordinary viscose loses roughly half its strength when wet, so it needs gentle handling. Modal and lyocell were developed in part to fix this, and later chapters cover them.
Abrasion, pilling and the strong-fibre trap
Abrasion resistance is how well a fibre survives rubbing. Nylon is exceptional here, which is why it is used in hosiery and outerwear shells. Polyester is also good.
Pilling is the formation of small balls of tangled fibre on the surface. It starts when loose fibre ends migrate out of the yarn and tangle. A weak fibre breaks off the ball, so the pill disappears. A strong fibre holds it. That is why polyester and nylon blends pill more visibly than wool or cotton of the same construction. High strength can make a garment look worse sooner, even though it lasts longer.
Elasticity and recovery
Three terms are often mixed up:
- Extensibility is how far a fibre stretches before breaking.
- Elasticity is the ability to return to the original length after the load is removed.
- Resilience is the ability to recover from bending, creasing or compression.
A fibre can stretch a lot and recover poorly. Cotton is an example. Wool stretches and recovers well because of the crimped, coiled structure of its protein chains, which uncoil under load and then spring back. Elastane (spandex) can extend several hundred percent and snap back because of its segmented polymer structure, with rigid and flexible segments. Chapter material on synthetics covers this in detail.
Crease behaviour follows resilience. Linen and cotton crease easily because hydrogen bonds between cellulose chains lock the fibre into a new shape when it is bent and damp. Wool and polyester resist creasing. Polyester can be heat-set, which means it keeps a pleat or shape through repeated washes.
| Fibre | Elastic recovery | Crease resistance |
|---|---|---|
| Elastane | Excellent | Excellent |
| Wool | Very good | Good |
| Nylon | Good | Fair |
| Polyester | Good | Very good |
| Silk | Fair | Fair |
| Cotton | Poor | Poor |
| Linen | Poor | Very poor |
| Viscose | Poor | Poor |
Heat behaviour
Heat sets the limits for washing, drying and ironing. Fibres respond in two broad ways.
Thermoplastic fibres
Thermoplastic fibres soften and then melt when heated. They are the synthetics: polyester, nylon, acrylic and elastane. The glass transition temperature is the point where the amorphous regions soften enough to be reshaped. Heat-setting uses this to fix pleats, and it is also why a hot iron leaves a shiny patch or a hole.
| Fibre | Approximate melting or decomposition behaviour |
|---|---|
| Polyester | Melts around 250–260 °C |
| Nylon 6,6 | Melts around 255 °C |
| Nylon 6 | Melts around 215–220 °C |
| Acrylic | Softens, then decomposes; no sharp melt |
| Elastane | Degrades around 150–200 °C range of heat damage |
These are indicative values. Safe iron settings are far below melting points because softening starts earlier.
Non-thermoplastic fibres
Cotton, linen, viscose, wool and silk do not melt. They char and decompose at high temperatures. Cellulosic fibres tolerate hot irons (cotton and linen the hottest). Protein fibres yellow and degrade at lower temperatures, so wool and silk need cooler pressing, with a damp cloth for wool.
Shrinkage
Shrinkage has three main causes, and they work differently:
- Relaxation shrinkage. Fibres and yarns held under tension during manufacture return to their relaxed state in the first wash. This is common in cotton and viscose.
- Felting shrinkage. Wool's surface scales interlock under heat, moisture and agitation, and the fabric tightens and thickens. It cannot be reversed.
- Heat shrinkage in synthetics. Heat-set fibres can shrink or distort if exposed to a temperature above the one used to set them.
Flammability
Cellulosic fibres burn readily and quickly. Wool and silk are harder to ignite and self-extinguish more easily. Synthetics melt and drip, which can cause serious burns by sticking to skin. The identification chapter returns to this because burn behaviour is also a test for fibre type.
Putting the properties together
Properties pull in different directions. A single fibre rarely wins on all four.
| Need | Look for | Watch for |
|---|---|---|
| Hot, humid comfort | High regain (cotton, linen, viscose) | Slow drying |
| Fast-drying sportswear | Low regain with a wicking construction | Odour retention, static |
| Hard wear | Nylon, polyester | Visible pilling |
| Shape retention | Wool, polyester, elastane | Heat limits, felting (wool) |
| Easy ironing | Polyester, wool | Melting at high iron settings |
This trade-off logic is the reason blends exist, a topic the later blending chapter takes up.
Common errors
- Equating regain with breathability. Regain describes vapour uptake. Breathability depends on fabric structure and air permeability too.
- Assuming strong means durable in appearance. Strong fibres hold pills and resist breakage, but the surface can look worn early.
- Treating all synthetics as non-absorbent. Nylon takes up several times more moisture than polyester.
- Treating "natural" as heat-safe. Wool felts and silk degrades at heat levels cotton tolerates.
- Applying cotton's wet strength to viscose. Both are cellulose, but viscose weakens sharply when wet.
Exercise
A shirt is sold as "100% polyester, ideal for hot, humid days because it wicks sweat." Using regain, wicking and heat behaviour, explain why the claim is partly right, and name one wear problem and one care rule you would expect.
Show answer
The claim is partly right. Polyester has a regain of about 0.4%, so it does not absorb water vapour into the fibre. It can still move liquid sweat along its surfaces and between fibres by wicking if the fabric is knitted or finished to do so, and it dries fast. The problem is that it takes up almost no vapour, so it can feel clammy while sweat is present, it builds static, and it can hold odour. The care rule: polyester is thermoplastic, so iron on a low setting (well below its melting point of roughly 250 °C) and avoid hot tumble drying that could distort heat-set shape.
Exercise
Why does a cotton shirt wash well at high temperature while a viscose blouse needs gentle handling, even though both are made of cellulose?
Show answer
Cotton gains strength when wet (about 105–110% of dry strength), so wet agitation does not weaken it. Ordinary viscose loses roughly 40–50% of its strength when wet, because its cellulose chains are shorter and less crystalline than cotton's, and water swells it and weakens it. A wet viscose fabric tears or stretches more easily, so it needs cool water, little agitation, and no wringing.